PC/ABS的縮水率在0.5%-0.7%。
常用縮水率
ABS 5‰
PS-HI 5‰
PC 6‰
POM 18-22‰
PMMA 5‰
SAN 5‰
AS 5‰
PA66 16‰
PPE 6‰
PPHOX 5‰
PPO 6‰
PSF 6‰
PPS 10‰
PHE 10‰
PES 0.6‰
PP 16‰
PBT 16‰
PC/ABS 5‰
FR2000 3.5‰
NL66+GF20 5‰
POM+GF25 6‰
PC+ASA 4‰
PC+ASA+CF10 1.25‰
PS+GF20 3‰
PPE+GF20 3.5‰
PPS- (GF+MD)65 1‰
PC+GF20 3.5‰
PBT+GF40 1.5‰
PBT+GF30 2‰
PPO+GF10 4‰
PC+GF30 2‰
POM+20%PTFE 15‰
PBT+ABS+GF30 1.5‰
PE 17‰
縮水率在6%左右的材料如果加玻璃纖維,其縮水率如下;
+GF10 3.5-4.5‰
+GF15 3.0-4.0‰
+GF20 2.5-3.5‰
+GF30 1.5-2.5‰
+GF40 1.0-2.0‰
>GF40 0.5-1.5‰
PC/ABS的縮水率在0.5%-0.7%。
常用縮水率
ABS 5‰
PS-HI 5‰
PC 6‰
POM 18-22‰
PMMA 5‰
SAN 5‰
AS 5‰
PA66 16‰
PPE 6‰
PPHOX 5‰
PPO 6‰
PSF 6‰
PPS 10‰
PHE 10‰
PES 0.6‰
PP 16‰
PBT 16‰
PC/ABS 5‰
FR2000 3.5‰
NL66+GF20 5‰
POM+GF25 6‰
PC+ASA 4‰
PC+ASA+CF10 1.25‰
PS+GF20 3‰
PPE+GF20 3.5‰
PPS- (GF+MD)65 1‰
PC+GF20 3.5‰
PBT+GF40 1.5‰
PBT+GF30 2‰
PPO+GF10 4‰
PC+GF30 2‰
POM+20%PTFE 15‰
PBT+ABS+GF30 1.5‰
PE 17‰
縮水率在6%左右的材料如果加玻璃纖維,其縮水率如下;
+GF10 3.5-4.5‰
+GF15 3.0-4.0‰
+GF20 2.5-3.5‰
+GF30 1.5-2.5‰
+GF40 1.0-2.0‰
>GF40 0.5-1.5‰